Default Anodising in Greater Sydney

I’m all but done with finishing up some brackets fabricated late last year by Slowsnake’s mate. Trimmed, drilled, tapped, edges broken… I want a simple protective clear matte anodising to stop them going “floury”. Anyone here had relatively recent dealings with a small works friendly anodiser?
Citroënbender is offline   Reply With Quote Multi-Quote with this Post
Old 12-07-2022, 06:25 PM   #2
Citroënbender
DIY Tragic
 
Citroënbender's Avatar
 
Join Date: Apr 2018
Location: Sydney, more than not. I hate it.
Posts: 21,043
Chairman's Award: Chairman's Award - Issue reason: Your outstanding contributions to this community have not gone unnoticed. IN my view you are a worthy recipient of the (rarely used) Chairman's Award. 
Default Re: Anodising in Greater Sydney

Another monologue.

Looks like Barry Ave Mortdale is still the go, haven’t been there since about 2007 but had a chat with their office (Vicki) and happy to deal with mug punters. Minimum charge $70+ now.
Citroënbender is offline   Reply With Quote Multi-Quote with this Post
This user likes this post:
Old 13-07-2022, 07:18 PM   #3
Citroënbender
DIY Tragic
 
Citroënbender's Avatar
 
Join Date: Apr 2018
Location: Sydney, more than not. I hate it.
Posts: 21,043
Chairman's Award: Chairman's Award - Issue reason: Your outstanding contributions to this community have not gone unnoticed. IN my view you are a worthy recipient of the (rarely used) Chairman's Award. 
Default Re: Anodising in Greater Sydney

Very thorough assessment of my submitted parts, I was cautioned liberally that the weld filler rod’s composition may cause discolouration if more than a hint of silicon or magnesium is in there. Estimated lead time on drop-ins, is around two weeks, possibly less.
Citroënbender is offline   Reply With Quote Multi-Quote with this Post
2 users like this post:
Old 21-07-2022, 12:29 PM   #4
Citroënbender
DIY Tragic
 
Citroënbender's Avatar
 
Join Date: Apr 2018
Location: Sydney, more than not. I hate it.
Posts: 21,043
Chairman's Award: Chairman's Award - Issue reason: Your outstanding contributions to this community have not gone unnoticed. IN my view you are a worthy recipient of the (rarely used) Chairman's Award. 
Default Re: Anodising in Greater Sydney

To wrap:

Parts dropped off 13/7, prepped for shop processes. Ready for pick-up 19/7.

That’s a good turnaround. My only regret - if you could call it so - was opting for a matte finish instead of semi-shiny. It’s slightly darker than surrounding bits of anodised aluminium.

I would go back; recommend them happily. The only thing I would do differently another time is bring in a finish sample, to be better guided on which process best matches.
Citroënbender is offline   Reply With Quote Multi-Quote with this Post
3 users like this post:
Reply


Forum Jump


All times are GMT +11. The time now is 06:40 AM.


Powered by vBulletin® Version 3.8.5
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Other than what is legally copyrighted by the respective owners, this site is copyright www.fordforums.com.au
Positive SSL